Scanning electron
microscopy (SEM) secondary electron images of surfaces on ferritic Fe-Cr-Al-Mo
alloy Kanthal APMT and Cr-Mo-V steel T91 (UNS: K90901) before and after oxidation
at 1200 C for 2 h in steam or air. Metadata detailing SEM imaging settings are
included for each photo.